Pick the right sealant for each joint, size the joint and backer rod, prep the surfaces, and tool a bead that stays bonded as the joint moves.

Table of contents

A bead of caulk is one of the first things a customer or inspector judges, and it keeps water and air out of the building. When caulk fails, the cause is rarely the gun. It is the wrong product, a joint with the wrong shape, or a surface that was dirty or wet.

Builders use "caulk" and "sealant" loosely. Caulk often means paintable acrylic latex for small interior gaps. Sealant means a product rated to stretch and compress as a joint moves. The label tells you which one you have.

What You Will Be Able to Do

  • Choose acrylic, silicone, polyurethane, hybrid or butyl for a given joint.
  • Read a sealant label for movement class, paintability and temperature.
  • Size a joint, choose a backer rod, and avoid three-sided adhesion.
  • Prepare, apply and tool a bead that bonds on both sides.
  • Know which gaps must never be sealed.

Sealant Types

Type Best for Watch out for
Acrylic latex Interior trim gaps, paint prep Low movement, shrinks in wide gaps
100 percent silicone Tubs, showers, glass, tile, metal Most cannot be painted
Polyurethane Concrete, masonry, exterior joints Odor, harder to tool, slow cure, primer on some surfaces
Hybrid (silyl-modified polymer) Siding, trim, windows, mixed materials Check paint and primer rules
Butyl Metal roofing, gutters, hidden laps Stays tacky, poor for painting

Acrylic latex is the painter's caulk. It cleans up with water and takes paint, often the same day. "Siliconized" versions are a bit more flexible, but they are still latex.

Silicone moves the most and holds up in sun and water, which makes it the standard for wet areas. Kitchen and bath versions add a mildew inhibitor. Silicone leaves a thin film that almost nothing bonds to, including new silicone, so removal and cleaning have to be thorough.

Polyurethane bonds well to concrete and masonry, and self-leveling grades flow into flat joints such as sidewalks. Hybrid sealants combine high movement with paintability, and some are labeled for damp surfaces.

Reading the Label

  • Movement class. Sealants that meet ASTM C920 are rated by how far they stretch and compress, as a percent of the joint's width. Class 25 handles plus or minus 25 percent, and Class 50 handles plus or minus 50 percent. Class 100/50 stretches 100 percent and compresses 50 percent.
  • Paintability, and whether it must cure first.
  • Interior or exterior use.
  • Temperature range for application.
  • Tooling time, which is how long you have before the surface skins over, and cure time.
  • Surfaces and primers the product is approved for.

Worked Example: Is the Joint Wide Enough?

A sealant can only stretch a fixed share of the joint width, so divide the expected movement by the movement class.

A butt joint in exterior trim will open and close 1/8 inch.

  • Class 25 sealant: 1/8 / 0.25 = 1/2 inch wide joint.
  • Class 50 sealant: 1/8 / 0.50 = 1/4 inch wide joint.

A 1/8-inch joint filled with Class 25 sealant would have to move 100 percent of its width, and it will tear. Widen the joint or use a higher class.

Where Each One Goes

Location Use Do not use
Interior trim, crown, casing Acrylic latex Silicone, if it will be painted
Tub, shower, sink, backsplash Silicone or kitchen and bath sealant Plain latex
Inside corners of tile, tile to tub Silicone or the tile maker's sealant Grout
Exterior trim and siding joints Hybrid or exterior elastomeric sealant Interior latex
Window and door perimeter The sealant the window maker approves Anything incompatible with the frame
Concrete joints, slab to foundation Polyurethane Latex
Metal roofing and gutter seams Butyl or the roofing maker's sealant Latex
Fire-rated penetrations Listed firestop sealant for the tested system Any standard caulk
Around flues and chimneys High-temperature sealant the maker names Standard caulk or foam

Gaps You Must Not Seal

Caulk is not flashing. Water that gets behind siding or trim has to drain back out, and sealing these gaps traps it and rots the wall.

  • The bottom edge of lap siding and shingles.
  • Weep holes in brick veneer and weep slots in window frames.
  • The bottom edge of metal flashing and drip caps.
  • A window's bottom flange where the instructions leave it open to drain.

Designing the Joint

A good sealant joint bonds on two sides only and stretches between them like a rubber band. If it also bonds to the back of the joint, called three-sided adhesion, it cannot stretch, and it tears as soon as the joint moves.

  • Shape. The ideal bead is thin in the middle and wide where it meets each side, like an hourglass.
  • Depth. A common rule is a width-to-depth ratio of about 2 to 1, with depth between 1/4 and 1/2 inch. The data sheet controls.
  • Width. Many exterior joints work best between 1/4 and 1/2 inch wide. Wider joints need the sealant maker's design.

Backer Rod and Bond Breaker

Backer rod is a round foam cord pushed into the joint before sealing. It sets the depth, gives you something to tool against, and keeps the sealant off the back.

  • Choose rod about 25 percent wider than the joint so it stays put.
  • Use closed-cell rod for most exterior joints. Do not puncture or stretch it. Gas escapes from a damaged rod and makes bubbles in the sealant.
  • Push it in with a blunt tool to an even depth.
  • Where a joint is too shallow for rod, use bond-breaker tape at the back.

Worked example. A joint between a slab and a foundation wall is 3/4 inch wide. At 2 to 1, the sealant should be about 3/8 inch deep. A rod 25 percent wider than 3/4 inch is about 15/16 inch, so use 1-inch rod set 3/8 inch below the surface.

Preparing the Surfaces

Most failures are adhesion failures, and prep decides adhesion.

  1. Remove old sealant with a knife or scraper. Old silicone needs the remover or solvent the maker names.
  2. Clean dust, loose paint, oil, soap scum and mildew from the joint faces.
  3. Dry the joint fully unless the product is labeled for damp surfaces.
  4. Prime when the data sheet calls for it, often on porous masonry and some metals and plastics.
  5. Check the temperature against the label. A joint sealed on a very hot or cold day starts at one end of its movement and has less room the other way.
  6. Set rod or bond breaker.
  7. Mask exposed joints with painter's tape for straight edges.

Applying and Tooling

  1. Cut the nozzle at an angle, a little smaller than the joint, and puncture the inner seal.
  2. Use a dripless gun, and release pressure at the end of each run.
  3. Hold the gun at about 45 degrees. Pushing the bead ahead of the nozzle packs it in, and pulling is easier on small interior gaps. Either way, fill the joint so the sealant touches both sides.
  4. Move at a steady speed in one continuous bead. Start and stop at corners, not mid-run.
  5. Tool the bead within the tooling time. Press it in and shape it concave with a tooling tool or spoon. Tooling drives the sealant against both faces.
  6. Pull the masking tape right after tooling, before the surface skins.
  7. Clean up before cure. Latex cleans with water. Silicone, polyurethane and hybrids need the solvent the label names.

A damp finger is fine for interior latex. On exterior and wet-area joints, use a tool, since skin oil and saliva can weaken the bond.

Paint only when the label allows. Polyurethane can take days to cure through, and paint applied early may crack. Standard silicone cannot be painted, so choose a paintable product first if paint is planned.

Tubs and Showers

  1. Remove all old caulk and mildew, clean, and let the joint dry fully, often overnight.
  2. Fill a tub with water so the joint is as open as it will be in use.
  3. Run silicone or a kitchen and bath sealant, and tool it.
  4. Leave the water in and keep the area dry until the label's cure time has passed.

Fixing Problems

Symptom Likely cause Fix
Bead peels off one side Dirty, wet or unprimed surface Remove, clean, prime, reseal
Split down the middle Three-sided adhesion or joint too narrow Add rod, widen joint, use higher class
Paint cracks over the bead Painted before cure Wait for cure, use flexible paint
Bubbles in the bead Punctured rod or moisture Undamaged closed-cell rod, dry joint
Black mildew in a shower Plain latex or trapped water Reseal with silicone
New bead peels in weeks Applied over old silicone Strip and clean with the maker's remover

Common Mistakes

Mistake What it costs
Sealing the bottom of siding or a weep Trapped water and rot
Thin smear over a wide joint Tears at the first cold snap
Standard caulk at a fire-rated penetration Failed inspection and lost fire rating
Skipping the tooling step A bead that never bonds to both sides

Working Safely

  • Read the safety data sheet. Some sealants, primers and removers need ventilation, gloves and eye protection.
  • Cut away from your hand when removing old sealant, and retract the blade when you set it down.
  • Set up the ladder or lift for exterior joints before you load the gun.

Check Your Understanding

1. A painter wants silicone along new baseboard so it will last. What do you tell them?

Use paintable acrylic latex. Standard silicone cannot be painted, and its residue makes later repairs hard.

2. A trim joint will move 1/8 inch, and the joint is 1/4 inch wide. Will Class 25 sealant work?

No. Class 25 handles 25 percent of 1/4 inch, which is 1/16 inch. Use Class 50 or widen the joint to 1/2 inch.

3. A sidewalk joint is 1/2 inch wide. How deep should the sealant be, and what goes behind it?

About 1/4 inch deep, at 2 to 1, over closed-cell backer rod about 5/8 inch wide.

4. A homeowner asks you to seal the bottom edges of their lap siding to stop drafts. What do you say?

No. Those edges have to drain, and sealing them traps water behind the siding. Air sealing belongs on the inside.

Key Takeaways

  • Match the product to the joint: latex inside, silicone in wet areas, polyurethane on concrete, hybrid or elastomeric outside.
  • The movement class must cover the joint's movement as a percent of its width.
  • Bond to two sides only, with backer rod or bond breaker, at about 2 to 1 width to depth.
  • Clean, dry and prime as the label says, then tool every bead.
  • Never seal joints that are meant to drain.