Injection Molding Basics

20 min read Training Guide

Explain how an injection molding machine makes a part, name the parts of the machine and mold, and stay safe around the clamp, hot barrel and hydraulics.

Table of contents

Injection molding makes plastic parts by pushing melted plastic into a steel mold under high pressure, cooling it and popping out the finished part. It is one of the most common ways to mass-produce plastic, from bottle caps and electrical connectors to dashboards and medical housings. A press can repeat the same cycle thousands of times a day. Your job as an operator is to keep that cycle steady, catch bad parts early and stay clear of a machine that can crush, burn and inject oil under your skin.

What You Will Be Able to Do

  • Describe the four phases of the molding cycle and explain why cooling takes the longest.
  • Name the main parts of the injection unit and say what the screw and check valve do.
  • Explain clamp tonnage and estimate it from a part's size.
  • Name the parts of a mold and tell the A side from the B side.
  • Spot the serious hazards at a press and what protects you from each one.

The Molding Cycle

Every part goes through the same four phases, one after the other. Then the cycle repeats.

1. Clamping

The two halves of the mold close and the clamp unit locks them with great force. The clamp has to hold the mold shut against the pressure of the plastic trying to push it open.

2. Injection

The screw drives forward like a plunger and pushes melted plastic through the nozzle and into the mold. This phase has two parts.

  • Fill: The screw moves forward at a set speed to fill the cavity. Fill usually takes 1 to 5 seconds.
  • Pack and hold: Plastic shrinks as it cools. After the cavity is nearly full, the screw keeps pressing to squeeze in a little more material and make up for that shrinkage. Pack pressure is usually lower than fill pressure, and it lasts until the gate freezes shut.

3. Cooling

Water flowing through channels in the mold pulls heat out of the plastic until the part is solid enough to handle. Cooling usually takes up the largest share of the cycle, often 50 to 80 percent of it. While the part cools, the screw turns and backs up, melting the next shot. This is called recovery.

The biggest factor in cooling time is wall thickness. Heat has to travel out through the plastic, and plastic conducts heat poorly. Cooling time rises with roughly the square of the thickness. If a wall of 0.080 inch needs 8 seconds of cooling, a wall of 0.160 inch needs about 32 seconds, not 16. The resin and the mold temperature also play a part.

4. Ejection

The mold opens and ejector pins push the part off. It drops into a bin or onto a conveyor, or a robot takes it out. Then the mold closes again.

Most parts cycle in 15 to 60 seconds. Thin-walled cups and lids can run in under 5 seconds, and thick structural parts may take 90 seconds or more.

The Injection Unit

The injection unit melts the plastic and pushes it into the mold.

  • Hopper: Holds the plastic pellets, called resin, and feeds them into the barrel by gravity. It may have a dryer or a blender for colorant attached.
  • Barrel: A heavy steel tube wrapped in electric heater bands. It usually has 3 to 5 temperature zones, controlled separately, and set to climb from the feed end toward the nozzle.
  • Screw: The heart of the unit. It has three jobs: it carries the pellets forward, helps melt them, and then acts as the ram that injects them into the mold. Most of the melting heat actually comes from friction as the screw turns.
  • Nozzle: The tip that presses against the mold's sprue bushing. It has to seal tight or plastic leaks out.
  • Check valve: Also called a non-return valve or check ring, this sits at the tip of the screw. It works like a one-way door. During recovery it is open, so melt can flow to the front of the screw. During injection it closes, so the melt goes into the mold instead of back along the screw.

The screw has three sections, each with its own job.

Section Flights What it does
Feed zone Deep Picks up pellets and moves them forward
Transition zone Getting shallower Compresses the plastic and adds friction heat
Metering zone Shallow Evens out the melt's temperature and thickness

The Clamp Unit

The clamp unit opens and closes the mold and holds it shut during injection.

  • Platens: Two large flat steel plates. The stationary platen holds one half of the mold, and the moving platen holds the other and travels back and forth.
  • Tie bars: Four steel bars that connect the platens and take the clamp load. Their spacing limits how big a mold will fit.
  • Ejector system: Cylinders or servo drives in the moving platen that push the ejector plate inside the mold.
Clamp type How it works Known for
Toggle A linkage driven by a cylinder Fast motion, tonnage set by linkage and die height
Direct hydraulic A large cylinder moves the platen Precise tonnage, simple mechanics
Electric (servo) Servo motors and ball screws Low energy use, precision

Clamp Tonnage

Clamp tonnage is the force that holds the mold closed, measured in tons. Presses run from about 50 tons for small connectors to 4,000 tons or more for bumpers and large appliance panels.

Melted plastic pushes outward on every square inch of the part it touches. If that push is greater than the clamp force, the mold halves separate a tiny amount and plastic squirts out between them. That thin extra plastic is called flash.

A common starting estimate is 2 to 5 tons for each square inch of projected area, depending on the resin and the wall thickness. Projected area is the part's outline as seen from the direction the mold opens. Worked example: a mold has four cavities, and each part is 6 inches by 5 inches.

  • Area of one part: 6 x 5 = 30 square inches.
  • Area of four parts: 30 x 4 = 120 square inches.
  • At 3 tons per square inch: 120 x 3 = 360 tons.

The setup sheet gives the real number for each mold, so use that when you have it.

The Mold

The mold, also called a tool, is a precision steel assembly with the shape of the part cut into it.

A Side and B Side

  • A side (cavity side): Usually the stationary half. It forms the outside, cosmetic face of the part and usually holds the sprue bushing.
  • B side (core side): Usually the moving half. It forms the inside features and carries the ejector system.

As the plastic cools, it shrinks tight onto the core. So when the mold opens, the part normally stays on the B side, right where the ejector pins can push it off.

How Plastic Gets to the Part

Plastic flows from the nozzle through the sprue, along the runners, and through a gate into the cavity.

  • Sprue: The first channel, running from the nozzle into the mold.
  • Runner: Channels that carry plastic from the sprue to each cavity.
  • Gate: The small opening between the runner and the cavity. It controls how plastic enters the part. Its size and location affect the fill pattern, the look of the part and its strength. Common types include edge, submarine (tunnel), pin and valve gates.
Runner type How it works Tradeoff
Cold runner Freezes with each shot and comes out with the part Runner must be reground or scrapped
Hot runner A heated manifold keeps the plastic melted No runner scrap and often a shorter cycle, but costs more to build and maintain

Cooling Channels and Vents

  • Cooling channels: Water passages through both mold halves. Oil is used for higher temperatures. Even flow matters, because uneven cooling leads to warped parts.
  • Vents: When plastic fills a closed cavity, the air in there has to go somewhere. Vents are very shallow grooves, usually 0.0005 to 0.002 inch deep, at the parting line and around ejector pins. They let air out but are too shallow for most plastic to enter. Without them, trapped air causes burn marks, unfilled spots and weak lines where flow fronts meet.
  • Parting line: The line where the two mold halves meet.
  • Ejector pins: Steel pins that push the part off the core.

What an Operator Does on a Shift

Duties vary by plant, but most operators do some or all of these.

  • Check that gates and safety devices work, as your procedure requires.
  • Keep the hopper or feed system supplied, using the correct resin lot.
  • Remove, trim and pack parts, and inspect them to the work instruction.
  • Watch for changes in cycle time, cushion (the small amount of plastic left in front of the screw) and part weight, and report them.
  • Record checks on the production log.
  • Keep the area clean.

A steady process stays steady. If a number on the screen changes, or a part looks different, something changed. Tell your process tech rather than waiting for a bin of scrap to prove it.

Safety at the Press

Keep every gate and guard working. OSHA's general machine guarding rule, 1910.212, applies to these machines, and the industry's safety standard is ANSI/PLASTICS B151.1 (the 2017 edition covers horizontal and vertical machines). OSHA's mechanical power press rule, 1910.217, is not the rule for injection molding machines. Your plant's procedures, based on these, are what you follow.

The Clamp Area

The mold closes with enough force to crush anything between the halves. Never reach into the mold area while the machine is in automatic. Test the safety gate at the start of each shift or as your procedure says: opening the gate must stop the clamp from moving. Report a gate or interlock that does not work, and do not run the machine. All safety devices should be checked on the schedule from the machine maker.

Warning: Never bypass a gate, interlock or light curtain, and never climb into a press or reach past a guard. For mold changes, repairs and other work between the platens, lock out the machine under your plant's energy control procedure (OSHA 1910.147). Hydraulic pressure, air, electricity and gravity can all move a platen or ejector. A short task that is routine to production, like clearing a part, is only exempt from lockout when your plant has a method that gives effective protection. Ask before you do it.

Heat

Barrels run at 400 to 600 degrees F or higher. Nozzles, barrels and fresh purge can all cause serious burns. Melted plastic sticks to skin and keeps burning. Purge is the plastic you shoot out into the open to clear the barrel, and a blob can stay hot inside long after the outside looks cool. When purging, wear heat-resistant gloves and a face shield, keep the purge guard closed, and stand to one side of the nozzle. Trapped gas can spit plastic out with no warning.

Hydraulics

Hydraulic oil often runs at 2,000 to 3,000 psi. A pinhole leak can shoot oil through skin. The wound may look small but it is a medical emergency, so get to a doctor right away and say it was an injection injury. Never check for a leak with your hand. Report leaks and worn hoses.

Fumes

Some resins give off dangerous gases when they overheat. Acetal (also called POM) gives off formaldehyde, and PVC gives off hydrogen chloride. Use the ventilation or local exhaust your plant has provided.

Warning: Acetal and PVC must never mix in a barrel. Even a little PVC can break acetal down fast, making gas and pressure that can blow melted plastic out of the machine. Clear the barrel fully and follow your plant's changeover rule between these resins.

Other Hazards

  • Pinch points: The mold, ejector plate and nozzle carriage all move. Keep your hands clear.
  • Robots and sprue pickers: Stay out of their reach and use their own guards.
  • Slips: Pellets on the floor roll like ball bearings, and oil and purge are slick too. Clean up right away.
  • Hot runner wiring: Water lines and heater wiring sit close together. Report leaks near electrical connections.

Common Mistakes

Mistake What it costs How to avoid it
Reaching in on a running press Crushed hand or arm Use the gate, follow the procedure
Skipping the gate test A failed interlock goes unnoticed Test it as your procedure says
Loading the wrong resin Scrap, possible barrel hazard Check the label against the job
Ignoring a small hydraulic leak Injection injury, slip, fire Report it now
Staying in front of the nozzle while purging Burns from spit plastic Stand to the side, shield on
Not reporting a changed number Hours of bad parts Tell the process tech early

Check Your Understanding

1. A new part has walls twice as thick as the old one. About how much longer will it need to cool?

About four times longer, because cooling time rises with roughly the square of the wall thickness. That is why cooling takes so much of the cycle.

2. During injection, melted plastic slips backward past the screw tip instead of going into the mold. Which part has likely failed, and what is its job?

The check valve. It should open during recovery to let melt pass forward and close during injection to stop backflow.

3. A mold has two cavities, and each part has a projected area of 25 square inches. Using 4 tons per square inch, what clamp force is needed?

Total area is 2 x 25 = 50 square inches. 50 x 4 = 200 tons. The mold's setup sheet still has the final say.

4. You see a fine mist from a hydraulic hose near the clamp. What do you do?

Stay clear and keep your hands away from it. A pinhole leak can inject oil into your body. Stop the machine as your procedure allows and report it right away.

5. The mold opens and the part has stayed on the moving half. Is that a problem?

No. That is the normal case. The part shrinks onto the core on the B side, where the ejector pins can push it off.

Key Takeaways

  • The cycle is clamp, inject (fill and pack), cool, eject. Cooling usually takes the longest.
  • The screw carries, melts and injects the plastic. The check valve stops it from flowing backward.
  • Clamp tonnage must beat the pressure inside the mold, or the mold opens and flashes.
  • The cavity is usually the A side, and the part usually stays on the B side core for ejection.
  • Guarding here falls under OSHA 1910.212 and ANSI/PLASTICS B151.1, with lockout under 1910.147.
  • Keep clear of the clamp, purge and hydraulic leaks, and never let acetal and PVC mix.